Solder Wire Total Products: 71
Filters
HARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.0625 in Weight 0.25 lb Melting Temperature (M...
View full DetailsHARRIS 40/60 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 40 Percent Tin 60 Percent Lead Wire Diameter 0.062 in Weight 1 lb Melting Temperature (Minimu...
View full DetailsHARRIS 60/40 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 60 PercentTin 40 Percent Lead Wire Diameter 0.03125 in Weight 16 oz Melting Temperature (Mini...
View full DetailsHARRIS Stay-Brite 8 Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 94 Percent Tin 6 Percent Silver Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Minimum) 4...
View full DetailsHARRIS Sterling Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 91 Percent Tin 4-5 Percent Copper 1 Percent Others Wire Diameter 0.118 in Weight 1 lb Melting Temp...
View full DetailsHARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Maxim...
View full DetailsHARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.1 in Weight 1 lb Melting Temperature (Maximum...
View full DetailsHARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Maxim...
View full DetailsHARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.0625 in Weight 1 lb Melting Temperature (Maxi...
View full DetailsHARRIS 97/3 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.03125 in Weight 1 lb Melting Temperature (Max...
View full DetailsHARRIS 40/60 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 40 Percent Tin 60 Percent Lead Wire Diameter 0.062 in Weight 1 lb Melting Temperature (Minimu...
View full DetailsHARRIS 60/40 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 60 PercentTin 40 Percent Lead Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Minimum...
View full DetailsHARRIS 60/40 Solder Wire
HARRISSolder Wire Form Flux-Cored Wire Material Composition 60 PercentTin 40 Percent Lead Wire Diameter 0.0625 in Weight 16 oz Melting Temperature (Minim...
View full DetailsHARRIS 50/50 Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 50 Percent Tin 50 Percent Lead Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Minimum) 36...
View full DetailsHARRIS 95/5 Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition Remainder Percent Tin 4.5-5.0 Percent Antimony Wire Diameter 0.118 in Weight 1 lb Melting Temperat...
View full DetailsHARRIS Premium Silver Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 95.6 Percent Tin 4 Percent Copper 0.4 Percent Silver Wire Diameter 0.118 in Weight 16 oz Melting T...
View full DetailsHARRIS Stay-Brite Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 96 Percent Tin 4 Percent Silver Wire Diameter 0.125 in Weight 1 lb Melting Temperature (Maximum) 4...
View full DetailsCHEMTRONICS Lead-Free Pocket Solder Wire
CHEMTRONICSSolder Wire Form Flux-Cored Wire Material Composition 96.5 Percent Tin 3 Percent Silver 0.5 Percent Copper Wire Diameter 0.04 in Weight 0.6 oz Melt...
View full DetailsAMERICAN BEAUTY Lead Free Solder Wire
AMERICAN BEAUTYSolder Wire Form Flux-Cored Wire Material Composition 97 Percent Tin 3 Percent Copper Wire Diameter 0.093 in Weight 0.25 lb Melting Temperature (Mi...
View full DetailsAMERICAN BEAUTY Lead Free Solder Wire
AMERICAN BEAUTYSolder Wire Form Flux-Cored Wire Material Composition 96.5 Percent Tin 3 Percent Silver 0.5 Percent Copper Wire Diameter 0.032 in Weight 11 g Melti...
View full DetailsOATEY 95/5 Solder Wire
OATEYSolder Wire Form Solid Wire Material Composition 95 Percent Tin 5 Percent Antimony Wire Diameter 0.117 in Weight 1.05 lb Melting Temperature (Minim...
View full DetailsHARRIS Stay-Brite Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 96 Percent Tin 4 Percent Silver Wire Diameter 0.125 in Weight 8 oz Melting Temperature (Maximum) 4...
View full DetailsHARRIS Bridgit Solder Wire
HARRISSolder Wire Form Solid Wire Material Composition 0.05-0.15 Percent Silver 0.05-2 Percent Nickel 2.5-3.5 Percent Copper 4.5-5.5 Percent Antimony Tin...
View full DetailsSolder Wire
WELLERSolder Wire Form Flux-Cored Wire Material Composition 99.3 Percent Tin 0.6 Percent Copper 0.05 Percent Nickel Wire Diameter 1 mm Weight 100 g Melti...
View full Details